The local priority corrosion of sintered MgO at the interface of molten slag ( SiO_2-FeO-CaO) and matte ( FeS-Cu_2S) was studied by the crucible method and high temperature X-ray video and radiographic technique. 采用坩埚法,借助自行设计的高温X射线透射影槐设备,通过X射线照像及电视观察,研究了烧结MgO材料在炉渣(SiO2-FeO-CaO)与冰铜(FeS-Cu2S)界面区局部优先侵蚀过程。
Sintered Crucible Coatings for Highly Undercooled CuNiFe Alloys 获得Cu-Ni-Fe熔体深过冷的烧结坩埚涂层